23.7: Magnetic Properties of Matter

Physics: A Foundation for Scientists and Engineers · LibreTexts

0%

Contents

    Text

    Size
    100%
    Theme
    Typeface
    Line length
    Spacing

    Read aloud

    How

    Speed: 1×
    Light up
    Highlight

    Symbols: Mulberry Symbols, © 2018–2026 Steve Lee, CC BY-SA 4.0 (licence, the set), the site's own copies.

    From LibreTexts, under CC BY 4.0, as the source states it; its equations are written in TeX, which the PDF shows typeset. This page at LibreTexts.

    23.7: Magnetic Properties of Matter

    A bar magnet has no wires and no battery. If every magnetic field comes from moving charge, where are the currents in a magnet? The answer lies in its atoms, and a full account of it requires the quantum mechanics of Part III. But the main ideas can be seen with a simple model.

    Magnetism and Atoms

    An electron in a circular orbit around a nucleus, drawn in perspective as a horizontal ellipse.
    Figure 23.13. An orbiting electron is a tiny current loop. Because its charge is negative, the current circulates opposite to its motion, and its magnetic moment points opposite to its angular momentum.
    Figure descriptionAn electron in a circular orbit around a nucleus, drawn in perspective as a horizontal ellipse. The electron moves counterclockwise when seen from above, so at the front of the orbit its velocity points to the right, while the conventional current, opposite to the electron's motion, circulates clockwise. The orbital angular momentum L points straight up from the nucleus, and the magnetic moment mu points straight down.

    Orbital magnetic moment. Picture an electron moving in a circular orbit of radius \(r\) with speed \(v\) around a nucleus (Figure 23.13). It passes any point of its orbit once each period \(T = 2\pi r/v\), so it constitutes a current loop with current \(I = e/T = ev/2\pi r\), circulating opposite to the electron’s motion because the electron is negative. The loop’s magnetic moment is

    \[\mu = IA = \frac{ev}{2\pi r}\,\pi r^2 = \frac{evr}{2}.\]

    The electron’s orbital angular momentum is \(L = m_evr\) (Chapter 11), so

    \[\vec{\mu} = -\frac{e}{2m_e}\vec{L}. \tag{23.12}\]

    The magnetic moment is proportional to the angular momentum, and opposite to it. This relation, derived from a classical picture, survives intact in quantum mechanics. What quantum mechanics adds is that angular momentum comes in units of \(\hbar = h/2\pi\) (Chapter 41). With \(L = \hbar\), the moment is the natural unit of atomic magnetism, the Bohr magneton:

    \[\mu_B = \frac{e\hbar}{2m_e} = 9.27\times 10^{-24}\,\mathrm{A\cdot m^2}. \tag{23.13}\]

    Spin magnetic moment. Electrons also have an intrinsic angular momentum, their spin (Chapter 41), and with it an intrinsic magnetic moment almost exactly equal to one Bohr magneton. It is not produced by any literal spinning; it is simply a property of the electron, like its charge and mass. Protons and neutrons have spin magnetic moments too, but roughly a thousand times smaller, because their mass is so much larger. Small as they are, nuclear moments are what an MRI scanner detects.

    Atoms as magnets. An atom’s total magnetic moment is the vector sum of the orbital and spin moments of all its electrons. In most atoms, electrons pair up with opposite spins and opposite orbital motions, and their moments cancel. Atoms with completed electron shells, such as helium and neon, have no net moment at all. Atoms with unpaired electrons, such as iron, cobalt, nickel, and the rare earths, have permanent moments of a few Bohr magnetons. In a bulk material, what matters is the magnetization \(\vec{M}\), the net magnetic moment per unit volume. Its unit is \(\,\mathrm{A\cdot m^2/m^3} = \,\mathrm{A/m}\).

    Example 23.9: The magnetization of iron

    Iron has \(8.5\times 10^{28}\,\mathrm{atoms/m^3}\), and each atom has a magnetic moment of about \(2.2\mu_B\). If all the moments are aligned, what is the magnetization, and what field \(\mu_0 M\) does it correspond to?

    Solution

    \[M = n\mu = (8.5\times10^{28})(2.2)(9.27\times10^{-24}) = \boxed{1.7\times 10^{6}\,\mathrm{A/m}}.\]

    The corresponding field is \(\mu_0 M = (4\pi\times10^{-7})(1.7\times10^{6}) = \boxed{2.2\,\mathrm{T}}\). This is close to the measured saturation field of iron, about \(2.1\,\mathrm{T}\). A solenoid would need \(n I = M = 1.7\) million ampere-turns per meter to produce the same field with no iron at all. Aligned atomic moments are an enormously concentrated source of magnetic field.

    Diamagnetism vs. Paramagnetism vs. Ferromagnetism

    Put a material inside a solenoid, and the field changes. If \(\vec{B}_0\) is the field that the solenoid’s current alone produces, the material contributes its own field \(\mu_0\vec{M}\), and the total is \(\vec{B} = \vec{B}_0 + \mu_0\vec{M}\). For most materials the magnetization is proportional to the applied field,

    \[\vec{M} = \chi_m\,\frac{\vec{B}_0}{\mu_0}, \qquad \vec{B} = (1 + \chi_m)\vec{B}_0, \tag{23.14}\]

    where the dimensionless constant \(\chi_m\) is the magnetic susceptibility. (The combination \(\kappa_m = 1 + \chi_m\) is the material’s relative permeability, the magnetic counterpart of the dielectric constant of Section 19.3.) Materials fall into three classes (Table 23.1).

    Table 23.1. Magnetic susceptibilities of some materials at room temperature (approximate; for ferromagnets, \(\chi_m\) depends on the field and on the sample’s history).
    ClassMaterialSusceptibility \(\chi_m\)
    DiamagneticWater\(-9.0\times 10^{-6}\)
    Copper\(-9.7\times 10^{-6}\)
    Bismuth\(-1.7\times 10^{-4}\)
    Pyrolytic graphite\(-4.5\times 10^{-4}\)
    Superconductor\(-1\)
    ParamagneticOxygen gas (STP)\(1.9\times 10^{-6}\)
    Aluminum\(2.2\times 10^{-5}\)
    Platinum\(2.7\times 10^{-4}\)
    Liquid oxygen\(3.5\times 10^{-3}\)
    FerromagneticNickelabout \(600\) (maximum)
    Iron (annealed)about \(5000\) (maximum)
    Mu-metalabout \(10^{5}\) (maximum)

    Diamagnetism. In a diamagnetic material, \(\chi_m\) is small and negative: the material’s magnetization opposes the applied field and weakens it slightly. Diamagnetism occurs in every material. An applied field slightly changes the orbital motion of every electron, and the change always produces a moment opposing the field (a consequence of Faraday’s law, Chapter 24). In most materials this effect is swamped by the others, but in materials whose atoms have no permanent moments, such as water, copper, and bismuth, it is all there is. A diamagnetic material is pushed away from a strong magnet, toward weaker field. The force is usually tiny, but in a field of \(16\,\mathrm{T}\) it is enough to levitate a living frog, whose water content makes it diamagnetic, as a famous experiment demonstrated in 1997. A superconductor is a perfect diamagnet, \(\chi_m = -1\): it expels magnetic fields completely, which is how a magnet can float above it.

    Paramagnetism. In a paramagnetic material, the atoms have permanent magnetic moments, but they point in random directions. An applied field tends to line them up, since that lowers their energy \(-\vec{\mu}\cdot\vec{B}\), but thermal agitation keeps knocking them out of alignment. The result is a small net magnetization along the field: \(\chi_m\) is small and positive, and a paramagnetic material is weakly attracted into a strong field. Because the competition is between alignment and thermal motion, the magnetization of a paramagnet is proportional to \(B_0/T\): it is stronger at low temperature. This is Curie’s law, discovered by Pierre Curie in 1895.

    Example 23.10: Why paramagnetism is weak

    Compare the magnetic energy of an atomic moment of one Bohr magneton in a field of \(1.0\,\mathrm{T}\) with the typical thermal energy \(k_BT\) at room temperature, \(300\,\mathrm{K}\).

    Solution

    The magnetic energy is at most \(\mu_BB = (9.27\times10^{-24})(1.0) = 9.3\times 10^{-24}\,\mathrm{J}\). The thermal energy is \(k_BT = (1.38\times10^{-23})(300) = 4.1\times 10^{-21}\,\mathrm{J}\) (Chapter 36). The ratio is

    \[\frac{\mu_BB}{k_BT} = \frac{9.3\times10^{-24}}{4.1\times10^{-21}} = \boxed{2.2\times 10^{-3}}.\]

    Thermal jostling is several hundred times more effective at scrambling the moments than the field is at aligning them, so only a fraction of a percent of the possible alignment survives. Cooling to liquid-helium temperature, \(4\,\mathrm{K}\), improves the ratio some seventy-five times, as Curie’s law predicts.

    Two panels of magnetic domains in a ferromagnet, each domain with its own magnetization arrow.
    Figure 23.14. Magnetic domains. (a) In unmagnetized iron, each domain is fully magnetized, but in different directions, so the net magnetization is small. (b) In an applied field, domains aligned with the field grow, the others shrink, and the net magnetization becomes large.
    Figure descriptionTwo panels showing magnetic domains in a piece of ferromagnetic material, drawn as a square divided into irregular regions, each containing an arrow showing its direction of magnetization. Panel a, unmagnetized: the arrows in the nine domains point in many different directions, so their magnetizations cancel. Panel b, in an applied field B zero pointing to the right: the domains magnetized to the right have grown and the others have shrunk, and most arrows now point to the right, giving a large net magnetization.
    A hysteresis loop: a graph of the magnetization M of a ferromagnet against the applied field B zero.
    Figure 23.15. A hysteresis loop. Starting from an unmagnetized sample (dashed), the magnetization rises to saturation. When the applied field is removed, a remanent magnetization remains; a reverse, coercive field is needed to remove it. Cycling the field traces out the loop.
    Figure descriptionA hysteresis loop: a graph of the magnetization M of a ferromagnet against the applied field B zero. A dashed initial magnetization curve rises from the origin to saturation at the upper right. As B zero is then reduced to zero, M follows an upper branch that stays high, crossing the vertical axis at the remanent magnetization. M reaches zero only at a negative applied field, the coercive field, and saturates in the opposite direction at the lower left. Increasing B zero again brings M up along a lower branch, symmetric to the upper one, so the curve forms a closed loop.

    Ferromagnetism. In iron, nickel, cobalt, and a few other materials and alloys, the magnetization is not weak at all: \(\chi_m\) can be thousands. These materials are ferromagnetic. In them a quantum-mechanical effect, the exchange interaction, makes the moments of neighboring atoms strongly prefer to point the same way. Within regions called magnetic domains, typically a fraction of a millimeter across, all the moments are aligned, and each domain is magnetized to saturation. But in an unmagnetized piece of iron, the domains point in different directions and their magnetizations cancel (Figure 23.14a). An applied field makes the domains aligned with it grow at the expense of the others, as the walls between domains move, and at higher fields it rotates whole domains into line (Figure 23.14b). A modest applied field can thus produce an enormous magnetization.

    Hysteresis and permanent magnets. The domain walls do not move freely; they catch on impurities and defects in the crystal. As a result, a ferromagnet’s magnetization depends not only on the applied field but on its history, a behavior called hysteresis (Figure 23.15). When the applied field is turned back to zero, the domains do not all return, and the material keeps a remanent magnetization: it has become a permanent magnet. A reverse field, the coercive field, is needed to bring the magnetization back to zero. “Hard” magnetic materials such as neodymium–iron–boron alloys have wide hysteresis loops and make strong permanent magnets. “Soft” materials such as annealed iron have narrow loops, lose their magnetization easily, and waste little energy when magnetized back and forth, so they are used in transformer cores and electromagnets. Hysteresis is also what makes magnetic data storage possible: the bits on a hard disk are tiny regions magnetized one way or the other, which stay that way until rewritten.

    The Curie temperature. Heat a ferromagnet and the thermal agitation eventually overwhelms the exchange interaction. Above a critical temperature, the Curie temperature, the domains disappear and the material becomes an ordinary paramagnet. For iron the Curie temperature is \(1043\,\mathrm{K}\) (\(770\,^{\circ}\mathrm{C}\)), for nickel \(627\,\mathrm{K}\), and for cobalt \(1388\,\mathrm{K}\); for gadolinium it is just \(293\,\mathrm{K}\), so a piece of gadolinium is ferromagnetic on a cool day and not on a warm one. When volcanic rock cools through its Curie temperature, its magnetic minerals freeze in the direction of Earth’s field at that moment. That fossil magnetism is the record of the reversals of Earth’s field mentioned in Chapter 22, and it provided some of the key evidence for plate tectonics.

    Checkpoint 23.5

    (a) A piece of aluminum and a piece of bismuth are held near the pole of a strong magnet. Which is attracted, and which repelled? (b) Why does hammering or heating a permanent magnet weaken it? (c) Why are transformer cores made of soft rather than hard magnetic material?

    Answer

    Answers to Checkpoints

    Checkpoint 23.5. (a) Aluminum is paramagnetic, so it is weakly attracted to the pole. Bismuth is diamagnetic (strongly so, for a diamagnet), so it is weakly repelled. Both effects are far too small to notice without a strong magnet. (b) A permanent magnet is strong because its domains are aligned. Hammering jolts the domain walls loose so that domains can flip into random orientations, and heating adds thermal agitation that does the same; above the Curie temperature, ferromagnetism disappears altogether. (c) A transformer’s field reverses direction many times a second. A soft magnetic material is easily magnetized and demagnetized, with a narrow hysteresis loop, so little energy is lost as heat in each cycle. A hard material, with its wide loop, would waste a great deal of energy.


    This page titled 23.7: Magnetic Properties of Matter was last modified on Thu, 12 Nov 2026 04:26:51 GMT and is shared under a CC BY 4.0 license and was authored, remixed, and/or curated by Michael Ragsdale.